HASTELLOY B2 UNS N10665 W.NR.2.4617
Himiki düzümi
Garyndy | elementi | C | Si | Mn | S | P | Ni | Cr | Mo | Fe | Co |
Garyndy B2 | Min | 26.0 | |||||||||
Maks | 0.02 | 0.10 | 1.00 | 0.03 | 0.04 | Balans | 1.0 | 30.0 | 2.0 | 1.0 |
Mehaniki aýratynlyklary
Aolly ýagdaýy | Dartyş güýji Rm Mpa Min | Hasyl beriň RP 0. 2 Mpa Min | Uzalma 5% Min |
Çözgüt | 745 | 325 | 40 |
Fiziki aýratynlyklar
Dykyzlygy g / sm3 | Eriş nokady ℃ |
9.2 | 1330 ~ 1380 |
Standart
Çybyk, bar, sim we ýasama aksiýa- ASTM B 335 (Rod, Bar), ASTM B 564 (Forging), ASTM B 366 (Fiting)
Tabak, list we zolak- ASTM B 333
Turbalar we turbalar- ASTM B 622 (bökdençsiz) ASTM B 619 / B626 (Kebşirlenen turba)
Hastelloý B2-iň aýratynlyklary
Stress Poslama poslama döwülmegine we çukuryna uly garşylyk
Hyd Wodorod hlorid, kükürt, sirke we fosfor kislotalary ýaly şertleri azaltmaga ep-esli garşylyk
All hydhli konsentrasiýalarda we temperaturalarda gidroklor turşusyna garşylyk
● Öňki: INCONEL® garyndysy C-276 UNS N10276 / W.Nr.2.4819
● Indiki: HASTELLOY B-3 UNS N10675 / W.Nr.2.4600
Näme üçin bizi saýlaň:
1. Professional gözleg we barlag topary
Programma synagy goldawy, birnäçe synag gurallary barada alada etmezligiňizi üpjün edýär.
2. Önüm marketing hyzmatdaşlygy
Önümler dünýäniň köp ýurtlaryna satylýar.
3. Hiliň berk gözegçiligi
4. Durnukly gowşuryş wagty we sargytlary gowşurmagyň wagtyna gözegçilik.
Biz professional topar, agzalarymyzyň halkara söwdasynda köp ýyllyk tejribesi bar.Biz ylham we täzeliklerden doly ýaş topar.Biz bagyşlanan topar.Müşderileri kanagatlandyrmak we olaryň ynamyny gazanmak üçin ökde önümleri ulanýarys.Biz düýş görýän topar.Biziň umumy arzuwymyz, müşderilere iň ygtybarly önümler bermek we bilelikde gowulaşmak.Bize ynan, ýeňiş gazan.