Products

  • SUPER DUPLEX S32760 / F55 / 1.4501

    Super Duplex S32760/ F55 , Super Duplex Alloy UNS S32760 (F55 / 1.4501) has excellent resistance Pitting and Crevice Corrosion in seawater at elevated temperatures, supplied with a PREN 40<( Pitting Resistance Eqv) . Excellent resistance to SCC ( Stress Corrosion Cracking) in Sour and Chloride environments .

  • 17-7 Steel Strip, Coil, Foil, Wire, AMS 5528 (CONDA), AMS 5529 (COND C), ASTM A693, MIL-S25043

    ● Springs
    ● Washers
    ● Clips
    ●Surgical parts
    ● Blades
    ● Bellows
    ● Honeycomb

  • Hastelloy B

    Hastelloy B is a solid solution strengthened, nickel-molybdenum alloy, with significant resistance to reducing environments like hydrogen chloride gas, and sulfuric, acetic and phosphoric acids. Molybdenum is the primary alloying element which provides significant corrosion resistance to reducing environments. This nickel steel alloy can be used in the as-welded condition because it resists the formation of grain-boundary carbide precipitates in the weld heat-affected zone.

    This nickel alloy provides excellent resistance to hydrochloric acid at all concentrations and temperatures. In additions, Hastelloy B2 has excellent resistance to pitting, stress corrosion cracking and to knife-line and heat-affected zone attack. Alloy B provides resistance to pure sulfuric acid and a number of non-oxidizing acids.

  • Monel 400 Uns N04400 W.Nr. 2.4360 And 2.4361

    MONEL nickel-copper alloy 400 (UNS N04400) is a solid-solution alloy that can be hardened only by cold working. It has high strength and toughness over a wide temperature range and excellent resistance to many corrosive environments. Alloy 400 is widely used in many fields, especially marine and chemical processing. Typical applications are valves and pumps; pump and propeller shafts; marine fixtures and fasteners; electrical and electronic components; springs; chemical processing equipment; gasoline and fresh water tanks; crude petroleum stills, process vessels and piping; boiler feed water heaters and other heat exchangers; and deaerating heaters.Chemical Compositions

  • Nimonic

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Cu Ti Al Co other no greater than Nimonic90 0.13 1 1 0.015 18~21 base ≤1.5 ≤0.2 2~3 1~2 15~21 lead≤0.002      B≤0.02        Zr≤0.15 Nimonic91 0.1 1 1 0.015 27~30 base ≤1 ≤0.5 1.9~2.7 0.9~1.5 19~21 Nb0.4~1.1  B0.002~0.01  Zr≤0.1 Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/...
  • ALLOY 825 MATERIAL DATA SHEETS

    Sandmeyer Steel Company stocks Alloy 825 nickel alloy plate in thicknesses from .1875″ (4.8mm) through 2.00″ (50.8mm) for corrosion resistant applications in the air pollution control, chemical and petrochemical, food processing, nuclear, offshore oil and gas production, ore processing, petroleum refining, steel pickling and waste disposal industries.

  • High Temperature Alloy

    Application Chemistry Typical Carbon  0.080 max Manganese  2.00 max Silicon  0.75 max Chromium  24.00- 26.00 Nickel  19.00- 22.00 Molybdenum  0.75 max Phosphorus  0.040 max Physical Properties Density  0.29 lbs/in³ 9.01 g/cm³ Electrical Resistivity  microhm-in (microhm-cm)  68°F (20°C)  37.0 (94.0) Specific Heat  BTU/lb/°F (kJ/kg•K)  32-212°F (0-100°C)  0.12 (0.50) Thermal Conductivity  BTU/hr/ft²/ft/°F (W/m•K) At 212°F (100°C)  8....
  • Nitronic

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Fe Mo Ti Cu Nb N other no greater than Nitronic50 0.06 1 4~6 0.03 0.04 20.5~23.5 11.5~13.5 base 1.5~3 - - 0.1~0.3 0.2~0.4 - Nitronic60 0.1 3.5~4.5 7~9 0.03 0.04 16~18 8~9 base — — — — 0.08~0.18 - Alloy property minimum Grade state tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% B...
  • 17-4PH Material Data Sheet

    International identifiers

    AISI 630, ASTM A564-89 17-4PH, JIS SCS24 / SUS630, AFNOR Z7CNU15-05 / Z7CNU17-04

  • High Precision Alloy

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu Fe Al Co Ti no greater than 1J50 0.03 0.15~0.3 0.3~0.6 0.02 0.02 - 49.5~50.5 - ≤0.2 base — — — 1J79 0.03 0.3~0.5 0.6~1.1 0.02 0.02 - 78.5~80.5 3.8~4.1 ≤0.2 base — — — 3J53 0.05 0.8 0.8 0.02 0.02 5.2~5.8 41.5~43 0.7~0.9 — base 0.5~0.8 — 2.3~2.7 4J29 0.03 0.3 0.5 0.02 0.02 ...
  • Nickel

    High Temperature Alloy Chemical composition Grade Ni Fe Cu C Mn S Si Nickel200 99 ≤0.4 ≤0.25 ≤0.15 ≤0.35 ≤0.01 ≤0.35 Nickel201 99 ≤0.4 ≤0.25 ≤0.02 ≤0.35 ≤0.01 ≤0.35 Alloy property minimum product form condition tensile strength RmN/m㎡ Yield Strength Rp0.2N/m㎡ Elongation As% Brinell hardness HB stick and strip hot rolled 60~85 15~45 35~55 45~80 stick and strip cold drawn or annealed 55~75 15...
  • Biphase Stainless Steel

    High Temperature Alloy Chemical composition Grade C Si Mn S P Cr Ni Mo Cu N W other no greater than F51 0.03 1 2 0.02 0.03 21~23 4.5~6.5 2.5~3.5 - 0.08~0.2 - - F53 0.03 0.8 1.2 0.02 0.035 24~26 6~8 3~5 ≤0.5 0.24~0.32 — - F55 0.03 1 1 0.01 0.03 24~26 6~8 3~4 0.5~1 0.2~0.3 0.5~1 - 329 0.08 1 1.5 0.03 0.035 23~28 3~6 1~3 - - - - A4 ...
123 Next > >> Page 1 / 3